For our full range of products and services, choose the relevant catalogue.
A380 Aluminum Casting Alloy
Chemical Composition
| Element | Symbol | Range / limit % |
|---|---|---|
| Silicon | Si | 7.5–9.5 |
| Copper | Cu | 3.0–4.0 |
| Iron | Fe | 1.3 max |
| Zinc | Zn | 3.0 max |
| Manganese | Mn | 0.50 max |
| Magnesium | Mg | 0.10 max |
| Nickel | Ni | 0.50 max |
| Tin | Sn | 0.35 max |
| Others, total | — | 0.50 max |
| Aluminum | Al | Balance |
Mechanical Properties
| Property | Metric | Imperial |
|---|---|---|
| Tensile Strength, typical | 324 MPa | 47 ksi |
| Yield Strength, typical | 159 MPa | 23 ksi |
| Elongation, typical | 3.5% | 3.5% |
| Hardness (Brinell), typical | 80 HB | 80 HB |
Composition to Aluminum Association A380.0 (NADCA permits up to 0.30% magnesium for die casting). Mechanical properties are typical values for die-cast A380 (NADCA), not specified minima.
Need a cast aluminum part? Kormax casts A356 in sand and investment castings.
Comparable and Related Specifications
The standards and grades below may have similar composition, properties or applications, but they should not be treated as direct equivalents without review. Chemistry, heat treatment, toughness requirements and testing provisions can differ between standards.
- Aluminum Association:
- A380.0
- UNS:
- A13800
- EN (EU):
- EN AC-46500 (AlSi9Cu3(Fe))
- JIS (Japanese Standard):
- ADC10
Applicable Casting Processes
Die casting (not offered by Kormax). For sand and investment castings, see A356.